Ịdozi ntụpọ ịgbado ọkụ na rọbọtị ịgbado ọkụna-agụnyekarị akụkụ ndị a:
1. Nkwalite oke:
Welding usoro parameters: Gbanwee ịgbado ọkụ ugbu a, voltaji, ọsọ, gas eruba ọnụego, electrode n'akuku na ndị ọzọ parameters ka dakọtara ịgbado ọkụ ihe, ọkpụrụkpụ, nkwonkwo ụdị, wdg ziri ezi oke ntọala nwere ike izere nsogbu ndị dị ka ịgbado ọkụ deviation, undercutting, porosity, na splashing. .
Siwing paramita: Maka ọnọdụ chọrọ ịgbado ọkụ, kwalite njupụta swing, ugboro ole, akụkụ mmalite na njedebe, wdg iji melite nhazi weld wee gbochie ntụpọ.
2. Welding egbe na workpiece n'ọnọdu:
TCP calibration: Gbaa mbọ hụ izi ezi nke ebe ịgbado ọkụ (TCP) iji zere mgbagha ịgbado ọkụ kpatara n'ọnọdu ezighi ezi.
● Ihe nrụnye arụ ọrụ: Gbaa mbọ hụ na ihe nrụnye ọrụ ahụ kwụsiri ike ma debe ya nke ọma ka ịzenarị ntụpọ ịgbado ọkụ kpatara nrụrụ workpiece n'oge usoro ịgbado ọkụ.
3. Teknụzụ nleba anya nke oke osimiri:
Ihe mmetụta a na-ahụ anya: nleba anya n'ezie ọnọdụ weld na udi site na iji ihe mmetụta visual ma ọ bụ laser, mgbanwe akpaaka nke trajectory egbe ịgbado ọkụ, na-ahụ na nsochi weld ziri ezi na ibelata ntụpọ.
Arc sensing: Site n'inye ozi nzaghachi dị ka arc voltaji na ugbu a,na ịgbado ọkụ parametersna egbe odidi na-dynamically gbanwee ime mgbanwe na elu nke workpiece, na-egbochi ịgbado ọkụ deviation na undercutting.
4. Nchekwa gas:
Ịdị ọcha gas na ọnụ ọgụgụ na-asọ asọ: Gbaa mbọ hụ na ịdị ọcha nke gas na-echebe (dị ka argon, carbon dioxide, wdg) na-emezu ihe ndị a chọrọ, ọnụego nrịba ahụ kwesịrị ekwesị, ma zere mmebi porosity ma ọ bụ oxidation nke kpatara nsogbu àgwà gas.
● Nhazi na nhicha mmiri: Jiri nozzles nke nha na ọdịdị kwesịrị ekwesị, na-ehicha mgbidi dị n'ime na ducts nke nozzles mgbe niile, hụ na gas na-ekpuchi welds ahụ nke ọma na nke ọma.
5. Ihe ịgbado ọkụ na pretreatment:
Nhọrọ waya ịgbado ọkụ: Họrọ wired ịgbado ọkụ nke dabara na ihe ndabere iji hụ na arụmọrụ ịgbado ọkụ dị mma yana ịdị mma weld.
● Nchacha arụ ọrụ: Wepụ ihe ndị na-adịghị ọcha dị ka ntụpọ mmanụ, nchara, na akpịrịkpa oxide n'elu ebe a na-arụ ọrụ iji hụ na ihe ịgbado ọkụ dị ọcha ma belata ntụpọ ịgbado ọkụ.
6. Mmemme na nhazi ụzọ:
Ụzọ ịgbado ọkụ: ezi uche na-ahazi ebe mmalite na njedebe, usoro, ọsọ, wdg nke ịgbado ọkụ ka ịzenarị mgbawa nke nrụgide nrụgide na-akpata ma hụ na eriri weld bụ otu na zuru oke.
● Zenarị nnyonye anya: Mgbe ị na-eme mmemme, tụlee mmekọrịta dị n'etiti egbe ịgbado ọkụ, workpiece, fixture, wdg. iji zere ndakọrịta ma ọ bụ nnyonye anya n'oge usoro ịgbado ọkụ.
7. Nleba anya na njikwa mma:
Nleba anya usoro: nleba anya n'ezie nke mgbanwe paramita na ịdị mma weld n'oge usoro ịgbado ọkụ site na iji sensọ, sistemu nnweta data, wdg, iji chọpụta ngwa ngwa na dozie nsogbu.
● Nnwale na-adịghị emebi emebi: Mgbe ịgbado ọkụ gachara, ultrasonic, radiographic, magnetic particle and other na-adịghị emebi emebi ga-eme iji kwado ịdị mma nke weld ahụ, a ga-arụzikwa welds na-erughị eru.
8. Ọzụzụ na nlekọta ndị mmadụ:
● Ọzụzụ ndị na-arụ ọrụ: Gbaa mbọ hụ na ndị na-arụ ọrụ maara usoro ịgbado ọkụ, ọrụ akụrụngwa, na nchọpụta nsogbu, nwere ike ịhazi ma dozie paramita nke ọma, wee dozie nsogbu ndị na-ebilite n'oge usoro ịgbado ọkụ.
● Ndozi akụrụngwa: Nleba anya mgbe niile, nyocha na nhazi nkeigwe ịgbado ọkụiji hụ na ha na-arụ ọrụ nke ọma.
Site na usoro zuru oke nke a kpọtụrụ aha n'elu, enwere ike ibelata ntụpọ ịgbado ọkụ nke robots ịgbado ọkụ na-emepụta nke ọma, enwere ike imeziwanye ogo ịgbado ọkụ na nrụpụta ọrụ.Ngwọta dị iche iche chọrọ nhazi na mmejuputa ahaziri iche dabere na ọnọdụ ịgbado ọkụ n'ezie, ụdị akụrụngwa, yana njirimara ntụpọ.